Chlorine Type LH-301 Macroporous Weakly Basic Anion Exchange Resin

Basic Information
Place of Origin: CHINA
Brand Name: MOSINTER
Certification: COA
Model Number: Oil Drilling Chemicals - 8
Minimum Order Quantity: 25KGS
Price: Negotiation
Packaging Details: 25KG/bag or as required
Delivery Time: Within 7 days
Payment Terms: L/C, T/T
Supply Ability: 200-300 MTS/month
Detail Information
Name: LH-301 Form: Particle
Color: Opacity Package: As Your Requirement
Advantage: Manufacturer Directly Supply Other Names: D301G

Product Description

LH-301 Macroporous weakly Basic Anion exchange resin Oil Drilling Chemicals

 

Description:

 

D301G is a kind of macrospore polystyrene ion exchange resin. It is used exclusively in gold extraction from alkali cyaniding mineral immersion liquid. Owing to the peculiar skeleton structure of polymer, this resin has excellent physical and
mechanical properties and extremely high wear resistant property. It has also a high
gold exchange speed and high adsorptive capacity. It can separate gold and other
metal ion well. The elution and reproduce is easy. So it is really an ideal material
for gold extraction in wet-process metallurgy.

 

Specifications:

 

Polymer structure Macrospore DVB cross linked polystyrene
Appearance Opacity spheroidal particle
Moisture content 45%-60%
Factory leaving pattern Chlorine type
Particle size 0.7mm<5%
0.7mm-1.7mm>95%
Hygro-apparent density 650-720kg/m3
Temperature limitation For free alkali type 60℃
For Chlorine type 100℃
PH Resin Stability 0-14

Absorption operation 0-11


Application:

 

D301G anion resin pretreatment
1, The resin is first loaded into the switch, the resin is sufficiently large backwash backwash to clarify the water, and then wash Taisho, but also to wash the water clarification.
2, Regenerated with 5% HCL, the amount of regeneration liquid is 2.5 times more than the volume of the resin must be regenerated flows, the reproduction end, soaks for 12-24 hours and then rinsed with pure water to near neutrality.
3, Then 4% NaOH solution was regenerated with regeneration is 2.5 times the amount of the liquid volume of the resin, 12-24 hours immersion , rinsed with pure water to meet the process requirements in use.

5) About water with resin regeneration treatment program as follows:
D301G anion resin pretreatment
1, the kettle (batch material) added 4% 4% NaOH solution regeneration, regeneration liquid than 20 cm liquid layer.
Second, soak 2 hours, stirring every half hour during 5-10 minutes.
Third, after soaking, put the net regeneration solution.
Fourth, repeat the operation a total of three times.
Five, three times after the end of regeneration, can be put to use.
2, one gram of gold probably needs 800-1200mm weak base anion resin adsorption.
(According to the actual situation, such as liquid gold concentration, etc.)
3, Russia, cycle: 100- 150 cycles. Broken rate of 40% or resin adsorption capacity decreased by 30% belongs to the scrap.
4, D301G resin or use after recovering 4% NaOH solution for use.

 

Our strengths:

 

We can customize according to customer's requirement

if you have any question pls mail us or call us

 

 

 

 

 

 

 

Contact Details
Fedor

Phone Number : +86 18989305995

WhatsApp : 18989305995